========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== You rang Modom? Water glass is a very strong solution of sodium meta silicate. I would think that since cuttlebone is a calcareous material, the outer parts of it would be converted to calcium silicate which is not so crumbly. This is what occurs when eggs are immersed in it; it gives them a siliceous coating that is impervious to air, and so they don't go rotten so quickly. it increases the strength of the shell too. I cannot see that there would be any deleterious fumes other than the burning off of the cuttlebone's organic material by hot metal. Another use for waterglass is to coat cement or concrete with it to make the surface more impervious to the carbon dioxide solution that comes dissolved in rain and eats it away over the years. Another but similar use is that if you have a concrete tank which leaks, put on a pair of rubber gloves, pour some cement powder into one hand, pour a little water glass into a hollow, mix as fast as you can and ram it into the leak for it will set hard in just a few seconds, even under water. -- Cheers for now, John Burgess; johnb AT ts.co.nz of Mapua Nelson NZ ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project