From: John Burgess
Date: Sun Mar 03 02:15:51 2002
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


>         BTW How do you dispose of the nitric acid when you are done?  I
>     hate to pour it down the drain.  I have been storing it in a jar
>     until I can find out where to dispose of it. 

    G'day 'Polymaid';  You can dispose of nitric acid by first
    neutralizing it with sodium bicarbonate - baking powder, or sodium
    carbonate - washing soda - until there is no more fizzing. Mix it
    with some inorganic material such as sand or even dry soil, but DO
    NOT use sawdust or shavings, for there is a possibility of it
    igniting spontaneously.    Spread the sand/neutralized mix on a non
    metallic surface - heavy polythene is OK - and allow it to dry
    thoroughly in the sun (if there is any where you are!).   Simply
    bundle it up and dispose of it in the usual way of solid waste.   It
    will contain sodium nitrate which is used as a fertilizer. -- Cheers
    for now, John Burgess;   johnb AT ts.co.nz of Mapua Nelson NZ 

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project