========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Marilyn, Water Glass is Sodium Silicate. I bought some for the same purpose at the corner drugstore here in Ketchikan (to stabilize a tufa stone mold, one of many projects I haven't gotten around to trying). I would think if they have it here, it should be available in most any drugstore/pharmacy. If not, I'm sure they could order it. My quart bottle cost about $14.00. Ofcourse, everything is expensive here (the classic explanation is shipping charges) The container says it is used for sealing concrete floors, water proofing, and gasket cement. Why do they sell it at a drugstore? I don't know. I have read in several places that it is used to stabilize stones such as turquoise as well. Good Luck, Chris Hanson Abo Originals Ketchikan, AK btw: Since I haven't used it yet, I haven't downloaded a MSDS but it does say to avoid contact with eyes and skin on the bottle. It would be wise to check out the safety info before using. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project