    Setting C.Z's is quite a common thing up here North of the 49th
    Parrallel (Canada) there are a few things you gotta watch out for
    while casting cz's. Don't let the little thingees touch while in the
    wax stage, why? the shrinkage will have them either touch and
    splinter or just turn into dust. CZ's do take the heat. Look into
    buying the better and stronger style of stones, askthe supplier if he
    would suggest a stone just for wax-gold-casting remember, DON'T LET
    THEM TOUCH..... AT ALL TIMES! Its the gold shrinkage that ruins your
    fine setting not necessarily, the heat!!!!! The Aqua, or Memeory Wax
    allows the stone to be inserted and the wax claws will expand and
    return to their shape after the stone is set. Now then,... after the
    casting, if you want to remove the fractured stone, a slight
    explosion occurs and splinters of cz can be felt escaping and hitting
     your eyes/face. I've seen this many, many times. I only wear glasses
    while doing this. The sudden hitting of the hammer to release this
    stone is at best, dangerous. Of course don't water quench the hot
    crucible. just a normal cooling will suffice. "Gerry, the
    cyber-setter !" "www.gemzdiamondsetting.com" gemz AT ican.net 

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project