From: Ettagale Date: Fri Mar 01 07:39:42 2002 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Platinum mining is not a byproduct of gold mining. It is found as a deposit on its own. In terms of mining processes, underground mining, whether gold, platinum or diamond, is very similar. In all cases, once the mining goes underground, shafts are sunk and then tunnels are constructed that follow the seam of the mineral being mined. Deep, narrow holes are drilled into the rock, sticks of dynamite are placed in the holes; the sticks are linked with wire. After the mine is cleared of all workers, the blast is set off and tons of ore are blasted loose. When the dust settles, literally, the next shift of workers descends and loads up the ore which is sent to the surface where the recovery process begins. Just thought you'd like to know from someone who has been underground at diamond, platinum and gold mines in South Africa. Ettagale Blauer ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project