From: Flynn, Don Date: Wed Feb 27 23:59:02 2002 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Kevin, > Problem was I didn't have any denatured alcohol. So I mixed my > boric acid with Everclear that I had left over from the days when > I drank occasionally. So, am I crazy or does anyone else use > Everclear also? I've work in the liquor and wine industry for over 30 yrs and way back when I graduated with a chemistry degree. One today, at work the fire marshal told us we would have to change all the fire protection within the warehouse because we carried Everclear in something like 190 proof this is 95 % ethanol. So we choose to dump the product. I took about four 750 ml bottles home and used them with Boric acid for antifirescale coating; it worked perfectly for this function. However, unless it's a "freebee" I'd use denatured ethanol every time. Don ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project