    Victoria, You are right it will be a bunch of trouble to take the
    stone out.You basically have to cut the stone out in your
    scenario.Then solder the bezel back together and reset the stone.I
    would strongly suggest NOT attempting to size this ring if you have
    as you say little experience sizing such things.The way I do it is to
    crank the oxy up on my torch and heat sink the stone by putting
    tweezers on each side of the stone.I aim the flame up towards the
    inside of the joint to be soldered.Pick up a ball of solder and lay
    the solder into the seem as the solder melts.I quickly put the ring
    on my ring mandrel to suck the heat away from the piece.It is very
    tricky to solder this way but it is the way I have soldered thousands
    of rings and it works for me.I wold not recommend it to someone with
    little experience and I would not practice on a very expensive
    stone.Another option is to have some one with a laser welder do it
    and charge the customer accordingly.regards J Morley Coyote Ridge
    Studio  

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project