    Virtually all emeralds sold today will either be oiled or fracture
    filled with one of a number of possible substances.  I can only
    recall seeing about a half doaen stones that weren't treated in the
    last twenty years and the only reason they weren't treated was
    because the treatment didn't take in the goods (they were from a
    Russian source)--in other words treatment was attempted but failed. 

    Today the differences in prices between treated emeralds is now
    often being judged by how much treatment is used but it is considered
    standard, acceptable trade practice to sell all emeralds with a
    treatment as long as it is disclosed. 

    I doubt very much that you will be able to find untreated stones
    anywhere. You just need to excersize the same type of precautions in
    wearing the emerald that you would with any delicate gemstone. 
    Incidentally, most stones can be retreated if for some reason the 
    treatment leaches out.

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project