    dear David, RMS is just an hour away in Clarkdale. We are casting on
    an irregular schedule. Usually 6/4. The darkness of sand blasted
    surfaces often relates to the consistency of the media. Is it new or
    old and broken down? What grit size etc. The darkness can be
    increased with a 17 to 22 volt dark blue anodized color added after
    blasting. As for the two alloys you mentioned they are close in
    Hardness, but 6/4 has a higher tensile and yield. the other
    consideration is 6/4 is common and made in many forms the other is
    not. I have heard of tension sets being made from Grade #2 seamless
    pipe. No one has written the book on tension settings in titanium.
    Everybody seems to be doing their own thing. Scratch resistant? Not
    really. More resistant then silver or gold? Yes. This stuff is not
    chrome. It is metal that has a tendency to gall, when it is highly
    polished scratches really stand out. I have always liked scratch
    brushed and glass bead surfaces. BIll

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project