    I'm not sure where to get these supplies, but I can tell you how to
    make your own stake for a lot cheaper.  Buy a small round bezel
    mandrel, and clamp the fat end into a vise.  Using your torch, heat
    an area about two thirds of the way up the mandrel (towards the fat
    end) until it's red hot.  Hold a piece of cut off metal pipe(or
    other non-valuable, sturdy metal tube) with pliers, slide it over
    the skinny end of the pipe until just before the red hot area, and
    use it to bend the mandrel the desired amount (35 degrees?).  Move
    the torch flame down an inch or two or wherever you want the next
    bend, and heat that area to red hot.  Bend the mandrel in the
    opposite direction.  Repeat this until you reach the end of the
    mandrel.  You can make deeper or shallower bends as you go for a
    surface variety.  I've found this works best with two people, one to
    hold the torch, and one to do the bending.  You don't want the torch
    on the metal while bending.  Good Luck, 

Michelle B. 

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project