tension rings have been appearing regularly on the market. From what
I have seen they are made from grade #2 Ti pipe. There are no real
rules or standards to go from. At least not written down anywhere.
Bill
Bill Seeley, President, Reactive Metals Studio, Inc.
Email- <reactive AT sedona.net>
Catalog web site- <www.reactivemetals.com>