    A little shameless self promotion for myself, but what the hell. 

    I only make titanium rings.  My rings are inlaid with gold, platinum,
    or silver and come in a variety of styles.  I do not know how to make
    jewelry, I only know how to make these titanium bands.  I am
    self-taught and invented a unique process that allows me to inlay any
    precious metal into a titanium band. 

    Each ring is machined to exact size from a solid bar of aerospace
    grade-5 titanium.  You cannot make titanium rings from titanium
    tubing.  I do this as a hobby for now, but it is rapidly becoming a
    full-time business.  If any of you store owners would like to carry my
    products, I am willing to sell at wholesale prices so you can sell at
    my web site prices. 

    Everybody please visit my web site and give me some feedback. 

    Thanks, 

Daniel J. Statman, Statman Designs
http://members.rennlist.com/statmandesigns
 

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project