>         I noticed in your commentary on vibro polishing you mention
>     steel   balls. Do you also have other shaped steel in there? 

    G'day;  No; I only use steel balls - a mixture of 1.5,  2.0 and 3.0
    mm.  We don't seem to be able to get the other shapes here.  I do find
    however, that although the insides of chain links do seem to get
    polished in my gadget, even the 1.5 mm balls can't get close enough to
    some parts of my jewellery, and leave a sort of very tiny 'tide mark'
    of unpolished silver.. I might try cutting off very small lengths of
    steel wire, but as I would need at least 300, it sounds a bit
    daunting. :-[     I tried broken up walnut shells, but they only
    pitted the job which was then rather useless. But because the smallest
    links  of my chains are made of rings made on a 2mm mandrel, they all
    come out beautifully burnished and polished. Isn't it lovely to get
    our Orchid 'fix' again!  I hope Hanuman is having a pleasant break,
    and many thanks to Dr E Aspler for taking over in the meanwhile. -- 


                /\      John Burgess
               / /
              / /      Johnb AT ts.co.nz
             / /__|\
            (_______)
 

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project