J Morley Saturday, February 05, 2000
   
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

    That depends.What type of stones are they?You said semi precious I
    would say you need to take them out.They are bezel set.If the bezel is
    in good shape you can put an xaxto blade ,a pointed one on the edge of
    the bezel and slowly and gently rock the edge of the bezel around the
    stone until it opens.Or you can take a very thin saw blade and make a
    very thin slice in the bezel  on each side of the stone.If the stones
    are soft making sure you don't cut them.Then peel the bezel back
    remove the stones solder the cuts by slipping a fresh piece of  bezel
    on edge into the cut you made clean excess with burr and wheels and
    then solder your wire and clean up and set stones.Or if you can bend
    the wire you have to solder away from the stones and you can solder it
    so the flame is not pointed in the direction of the stone and you can
    heat sink the stones and you feel confident and it is not a full moon
    and you have'nt broken any mirrors or walked under any ladders Do it! 
    J Morley Coyote Ridge Studio 