From: Nancy R. Garber Date: Tue Feb 01 18:46:07 2000 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I can't say much about anvils but I can tell you about Touchstone. They have just buildt a new blacksmith shop. I didn't see the new one but, the old one was extensive. You are in the woods up a mountain in a cabin. Each cabin does have electricity, screens, and some funiture. The food is ok. The classes are wonderful in all areas. The opprotunities besides metalsmithing and jewlery are excellent. They have many different kinds of kilns for pottery not just raku, salt and, normal reduction. (I was a potter for a good 10 years.) Watercolor, painting, printmaking ... all have wonderful teachers. The painting building is located next to and on top of a stream. You can even paint in the rain under the building, while looking at the stream with the interesting bridge. It takes me a while to drive to Touchstone from Detroit. I wish it were closer. Then I could take more classes there. I have gone to classes for 3 summers. The first 2 summers to take Marne Ryan's texturing metal and last year to take Steve Midgets mokume class. I only regret not taking Blaine's stone setting class. I am going back again. I wish I could split myself so I could be in all the classes at once. You do get to meet the other classes and people if you have time. I love seeing what the tin can class makes. Bobbie Hansen always is a stitch. He wrote the book on "Tin Can Art." I'm not sure of the title. It's the class with the most humor. Touchstone is located south of Pittsburg, Pa, if you're looking at a map. Nancy ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project