From: Skip Meister Date: Thu Nov 04 17:46:13 1999 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi, An ancient dental tech :o) once taught me how to fuse a small higher melting point piece of gold to a lower melting point piece. We took a piece of thick masonry with a smooth glaze on one side that fit flat against a concrete block and put them in the freezer overnight. The piece to be soldered to was put in a thin (1/4" thick piece of soldering investment) and also put into the freezer. When you are ready, you place the piece to be soldered in place and hold it with a little flux. Using a very hot flame, glance it on an angle until the surface of the invested metal begins to melt. Immediately get the torch away from it and voila it is stuck. You get only 1 try without starting over. Hope this is of some use. Regards, Skip ------------------------------------- Skip Meister hansgraf AT xnet.com Orchid Jewelry Listserve Member A day without sunshine is like night! N.R.A. Endowment "No man's life, liberty or fortune is safe...while our legislature is in session." Benjamin Franklin ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project