    The flux comes in a cylindrical 'can' about 4 1/2" tall  x 1 3/4"
    dia.  I have had mine for 12 years (about 5000 casting melts)  and
    there is about 1/3 of a 'can' left, so I don't use very much (three
    quick shakes per oz. of metal).  This flux also has borax in it.  The
    residue from the 'cleansing' ends up as a 'glass' on the bottom of
    the button.  Pickle removes it.  I can't remember the particulars of
    what the Ney metalurgist told me a zillion years ago, but I can even
    use this casting flux on my high heat gold alloys which are used for
    dental ceramic application.  *ANY* contamination, even finger (body)
    oils, is a delayed 'death sentence' which interferes with the
    ceramics chemically bonding to the metallic oxide layer.  This
    usually appears as a large 'air' bubble on the final glaze bake, as a
    'crater' through the porcelain down to bare metal, OR is one of the
    problems that causes the ceramics to shear cleanly off down to the
    metal substructure after the crown is cemented into the mouth. 

Regards,

Skip

-------------------------------------
Skip Meister
hansgraf AT xnet.com
Orchid Jewelry Listserve Member
A day without sunshine is like night!
N.R.A. Endowment  
"No man's life, liberty or fortune is safe...while our legislature is in session." 
Benjamin Franklin


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project