John Burgess......Large diameter drill bits are frequently tipped
with carbide. However small diameter drills are frequently solid
carbide. I cant tell you how small is small, but I own a 1/16 inch dia
solid carbide drill bit. Gosh it feels good to be able to add to your
vast information bank !!