Hi Rawennek Sorry to take so long.... I have used 32 gauge fine
silver wire and I have used in in the same manner that yarn is
used, I guess when you learn this early, it becomes almost second
nature. I am assuming you have done weaving. If you have, you
can do patterns using different colors of gold or combinsations
with silver or you can use stitches to show figures in relief.
I picle my silver to give it that ultra white appearance that we
use for filigree (?) . If you have any questions, or if I am
being vague, please feel free to contact me again. I will send
pictures of my, my mom's work or work from one of my relatives
soon. Thanks for asking. I guess I am freaking out. I am
working on my ppieces for next year slides and I hear some of you
are picking out the ones you have....Ayyyyyyy I am so behind
It will get better, I know. Elizabeth
Would you like to reach Members of the Ganoksin Project to educate
them about the wonderful array of supplies, services and products
you have to offer?
Please request a copy of the Ganoksin Media Kit if you would like
more indepth information regarding Ganoksin's advertising services.