Didn't mean to just send one line and yelling at that! You need to get your
mold as cold as possiable and scrape it with something semi sharp with out
cutting into the mold its self. It should clean up pretty easily. If you
can help it DON"T use any kind of petrolium product, as it will breakdown
your rubber. Try to find some mold release made for rubber spray some on
then shot some waxes!! clean it up as good as you can, then use some mold
release powder. Good luck!!