For a sharp corner, mark the inner surface  where you want the bend, then
score it with a triangular or square needle file....not too deep, but just
enough to get  a sort of miter cut. It will bend sharp and easy.  If  you
overdo it and weaken it, a trace of solder skillfully applied will restore
the strength to the crease. 