Re: [Orchid] Casting Problem
-> Navigate by Topic: [Thread Prev] [Thread Next]
-> Navigate by Date: [Message Prev] [Message Next]
-> Locate this message on the Date Tree or Thread Tree


AmberHumm Tuesday, November 04, 1997
   
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


    Bob The cracking in your casting could definately be caused by
    quenching to soon. Let it cool past the recomended red but not
    too long or the investment will be a pain to remove, however, I
    would rather spend a few extra min.  removing investment than
    trying to deal with a cracked piece. good luck! Amber