| A
Mineral may be defined as a homogenous substance produced by the
processes of inorganic nature having a chemical composition and physical
properties which are constant within narrow limits. Its structure is crystalline.
It is composed of the same substance throughout. Except for impurities
it has the same chemical formula for all specimens of the mineral. Its
atoms usually have a definite and ordered crystal structure. What makes
a mineral (or an organic product) a gemstone is cultural and partly subjective:
beauty, durability and rarity.
Minerals often occur in geometrical forms bounded by plane surfaces.
These are crystals and the internal structure determines properties which
allow the identification of the gem material; its differentiation from
other minerals, imitations and sometimes synthetics.
Crystals have:
1. An orderly and symmetrical atomic structure.
2. A definite external geometrical shape bounded by plane faces.
3. Physical (and optical) properties which vary with direction.
Glass has:
1. No regular atomic structure.
2. No tendency to assume a definite external shape.
3. Properties which are the same in all directions.
(the above derived from the British Gemmological Association's course
material. I strongly recommend their program to aspiring gemmologists)
Crystalline Material: Possesses the regular structure and directional
properties of a crystal but not the regular geometrical shape. Also called
massive. e.g. rose quartz.
Crypto-crystalline Material: Material which consists of a multitude
of tiny, often submicroscopic crystals. e.g. Chalcedony.
Symmetry:
Crystal symmetry refers to the balanced pattern of the atomic structure
which is reflected in the external (crystal) shape. Different species
vary in the symmetrical arrangement of faces. These arrangements have
certain 'planes' and 'axes' of symmetry. These form part of the definition
of the crystal system to which specific gemstones belong.
Plane of symmetry:
An imaginary plane dividing a body into two parts such that each is the
reflected image of the other. Crystals may have more than one plane of
symmetry. i.e. a cube has nine planes of symmetry.
Axis of symmetry:
An imaginary axis is placed through a perfect crystal so that during a
single rotation about this axis the outline of the crystal form appears
identically more than once; 2, 3, 4 or 6 times.
Centre of symmetry: (centro-symmetry)
Often present, it exists when every face of a perfect crystal is exactly
opposite a similar face on the other side of the crystal.
Crystal axes: (Crystallographic axes)
To describe crystals imaginary lines are used intersecting at 0 (the origin).
These are specific to the various crystal systems, intersecting at given
angles and being of given lengths specific to each crystal system.
Origin:
The intersection of the crystal axes.
Habit:
Gemstone species tend to occur in characteristic shapes which relate to
one or more of the forms common to the crystal system of the gemstone
in question. The crystal form or forms which a gemstone most often appear
are it's habit. e.g. diamond: octahedron, emerald: 6 sided prism.
Form:
Those faces of a crystal which are identically related to the crystal
axes. When the space so defined is completely enclosed (cube, octahedron)
it is a closed form. When identical faces do not completely enclose the
space (four or six sided prism; top and bottom open) it is an open form.
Twinned crystals: (compound crystals)
A twin is a single crystal composed of two or more parts with any part
in reversed structural orientation to the next, or interpenetrated.
Contact twin:
Sharing a common plane.
Interpenetrant twin:
Two individuals have grown from a common origin and appear to penetrate
each other. e.g. cross stones.
Lamellar twinning:
A series of contact twins often as extremely thin plates. Atoms in adjacent
sheets are reversed, i.e. alternate plates are in the same order. This
can give rise to special optical effects as in the feldspar labradorite.
Secondary twinning or parting:
The crystal is composed of very thin plates parallel to definite crystallographic
directions. e.g. ruby, this gives rise to 'false cleavage'.
CRYSTAL SYSTEMS
Cubic
Three crystal axes of equal length intersect at right angles to each other.
e.g. diamond, spinel, garnets. Tetragonal Three axes intersect at right
angles to each other. The vertical axis is of unequal length while the
two horizontal axes are of equal length. e.g. zircon, rutile.
Hexagonal
Four crystal axes. Three are of equal length and intersect at 60o to form
a horizontal plane which the fourth intersects at right angles. The vertical
fourth is of unequal length and forms an axis of 6-fold symmetry. e.g.
Beryl, apatite.
Trigonal
Four crystal axes. Three of equal length intersecting to form a horizontal
plane which is intersected at right angles by the fourth axis. The vertical
fourth is of unequal length and forms an axis of 3-fold symmetry. e.g.
quartz, corundum, tourmaline, dioptase, haematite.
Orthorhombic (Rhombic)
Three crystal axes of unequal length interest each other at right angles.
e.g. topaz, peridot, Chysoberyl, iolite, sinhalite, andalusite.
Monoclinic
Three axes. Two of unequal length intersect each other obliquely to form
a plane which is intersected by the vertical third (of unequal length)
at right angles. e.g. jadeite, nephrite, diopside, orthoclase feldspar,
serpentine, sphene, malachite, spodumene.
Triclinic
Three axes of unequal length intersect each other at oblique angles. e.g.
turquoise, labradorite.
NOTE:
The Gemological Institute of America (GIA)
system for crystal types differs from the above. Contact their web site
for information on their courses, books and so on.
CRYSTAL SYSTEM SYMMETRY
Singly Refractive: Amorphous -- no crystal structure
|
|
|
Optic Axis |
| Cubic |
9 planes |
4 3-fold |
-
|
|
13 axes |
3 4-fold |
-
|
|
a centre |
6 2-fold |
-
|
Doubly Refractive:
|
|
|
Optic Axis |
| Tetragonal |
5 planes |
1 4-fold |
uniaxial
|
|
5 axes |
4 2-fold |
|
|
a centre |
|
|
|
|
|
Optic Axis |
| Hexagonal |
7 planes |
6 2-fold |
uniaxial |
|
7 axes |
1 6-fold |
|
|
a centre |
|
|
|
|
|
Optic Axis |
| Trigonal |
3 planes |
3 2-fold |
uniaxial |
|
4 axes |
1 3-fold |
|
|
a centre |
|
|
|
|
|
Optic Axis |
| Orthorhombic |
3 planes |
3 2-fold |
biaxial |
|
a centre |
|
|
|
|
|
Optic Axis |
| Monoclinic |
1 axis |
|
biaxial |
|
a centre |
|
|
|
|
|
Optic Axis |
| Triclinic |
no planes |
|
biaxial |
|
no axes |
|
|
|
a centre |
|
|
Uniaxial
The optic axis of the crystal is parallel to the main crystal axis. One
direction of single refraction.
Biaxial
There are two directions of single refraction. (optic axes)
GEMSTONES BY CRYSTAL SYSTEM (major ones)
*Diamond simulants, man-made (U) = uniaxial, (B) = biaxial
Cubic
Diamond
Sodalite
Fluorite
Spinel
GGG *
Strontium Titanate*
Garnet
Yttrium Aluminate*
Lazurite (Lapis Lazuli)
Yttrium oxide*
Pyrites
Cubic Zirconia*
Tetragonal (U)
Idocrase
Rutile
Zircon
Trigonal (U)
Calcite (marble)
Quartz
Corundum
Rhodochrosite
Dioptase
Tourmaline
Hematite
Orthorhombic (B)
Andalusite
Marcasite
Chrysoberyl
Peridot
Danburite
Sinhalite
Enstatite
Staurolite
Iolite
Topaz
Kornerupine Zoisite
Monoclinic (B)
Azurite
Nephrite
Diopside
Orthoclase Feldspar
Epidote
Serpentine
Euclase
Sphene
Jadeite
Spodumene
Malachite
Triclinic (B)
Axinite
Kyanite
Microcline Feldspar
Plagioclase Feldspar
Rhodonite
Turquoise
*Diamond simulants, man-made (U) = uniaxial, (B) = biaxial
|