Making jewelry is
sometimes seen as a difficult or an expensive proposition. In reality a
basic metal working shop can be set up quite inexpensively. Cutting (separating
materials), soldered construction and finishing are the three main things
that jewellers do and what follows is a list of basic tools for doing these
things. One should be able to set up a basic shop for less than a hundred
dollars. Remember safety and make sure you have ventilation and use eye
protection when sawing and performing other potentially dangerous tasks,
it's not worth getting hurt because you took a short cut or didn't think.
There are numerous books one can start with depending upon the level
of jewelry making skills one aspires to,
Theory and Practice of Goldsmithing by Prof. Brepohl and Tim McCreight's the Complete
Metalsmith are excellent as
are many others that one can find at the library. Your local lapidary
club will often offer introductory classes in basic jewelry making far
more cheaply than any other route to learning. An approach which is less
hobby oriented and more of a professional pretraining is to use Alan Revere's Professional Goldsmithing book as
a text and go through it step by step, taking no account of time spent,
just concentrating on doing the best and most accurate job you can. If
you go through the projects in sequence and as carefully as possible one
would get a pretty good basic training. Revere's video series is also
good for those wanting slow, real time step by step tutoring on projects-you
could set up the DVD and (starting and stopping a bit) go through building
the items shown.
In any case the tools listed below should be readily obtainable and
affordable. You don't have to have the best to start out with. If you
want to by all means go all out in purchasing equipment but the tools
mentioned will get you rolling without breaking the bank. I am a firm
believer in fleas markets, second hand stores and lapidary clubs as sources
for used tools. Keep a tidy work place and organize from the start to
make your life easy.
You could begin by using an ordinary table (if you use your kitchen
remember to clean up and not mix food and metal working dusts and residues!).
If you want to set up a special place in your house for jewellery working
you will need a sturdy bench or table to work at and a good desk lamp
over your work place. The ventilation is needed primarily for soldering
and pickling. If you use an alum or vinegar pickle for cleaning metals
after soldering they put out far less noxious fumes than the normal jewellers
pickling cleaning solutions. Things to remember include that you don't
want to have to move out of your way to get a tool when working. Understand
your work space in relationship to your body. Move your body and arms
around while sitting in your favorite comfortable chair to work in. Usually
when seated in your chair your arms when straight out should rest on the
table top. You can of course start at another type of table-just don't
set yourself up for neck or back problems because of the height you are
working at. Get a feeling for how you are comfortable in your work space.
Then tools get positioned around your body space for maximum accessibility
in order of frequency of use. Watch how you move when you work. Notice
the natural paths you and your body take in space as you move at your
work. Position your tools along these paths in order of frequency of use,
ie when my right hand drops naturally down and hangs comfortably by my
side that is where my most used file is, about at palm height, nearby
are other tools. To put the file away the hand goes to its natural rest
position and lets go of it and it falls into a hole or slot in a piece
of wood attached to the bench to receive it. Kitchen magnetic strips and
old stereo speaker magnets attached to the wall or desk can be useful
holding devices. Again, getting organized and keeping a tidy work space
pays off in ease of working over the long run and is best learned as a
habit from the moment you start making jewelry - once you are used to
it it will be automatic and you will save hours of messing about by doing
so. Labelled plastic drawers for parts, tomato paste cans for files and
so on help to keep things where you can find them.
Jewelry making can be fun and even profitable once you start. My best
wishes to those starting on the adventure of jewelry making!
A list of useful tools follows.
Cutting, piercing, rough finishing tools A jewellers sawframe and a selection of blades; # 03, 02, 01, 0, 1. A
wooden bench pin (a piece of 1" board with a V-cut into it to clamp onto
a table) and a C clamp are good.
A beeswax chunk
for sawblade lubrication (slide it onto the blade to make sawing easier).
One each 6" flat and half round files, flea market versions are fine;
remember to put handles on them so you don't hurt your hands. Keep your
files from banging other tools for best results.
A set of needle files: if you look around you should find a set for
under four dollars these days.
A selection of emery papers, fine and medium grits at least.
A piece of medium emery paper is scored and tightly wound about a rectangular
cross sectioned wooden lath. The ends are thumb tacked tight. Different
shapes of lath and various grits are useful. Aluminum oxide holds up well.
This becomes a sanding stick which is used like a file to finish surfaces,
an extremely important finishing tool. Some people use a paint stick for
this.
A selection of drill bits and tools to drill with. A flexible shaft
or Dremel® like tool is best. An ordinary home electric drill will do
to start with. It helps to C-clamp metal so it can't move while drilling
it. A cardboard pad under the C clamp will protect the metal from damage
from the clamp.
A centre punch to start drill holes with; always start with a dent,
then use increasing sizes of drill bit until you get to the hole size
you want. Make it a habit to always take a larger drill bit in the hand
and take the burr off the edge of the drilled hole with it by twisting
it, this prevents all kinds of problems later. Also useful is a large
reamer for enlarging and tapering holes, it is found at the hardware store.
A pair of hand or aviation snips - if it is easier to use snips instead
of a jewellers saw then do so!
A small piece of flat steel (bottom of iron) to use under centre punch
and as an anvil surface.
A small ball peen hammer.
Some peel and stick white label stock, permanent marker, thin felt tips,
pencils etc for layout of drawings on metal. Photocopying and spray adhesive
work well for this kind of thing.
A large darning needle to use as a scribe for laying out lines for cutting
and so on.
A cold chisel if thick metal is to be cut. A hack saw is nice to have
around as well for such things.
A steel edged ruler is most useful. A plastic protractor and templates
for circles are nice to have.
A pair of dividers and/or Vernier callipers. Professionals have several
dividers on hand.
A machinists try square or an accurate small window frame brace (this
latter is a really cheap option) to measure and check right angles with.
A small vise can be useful.
Safety equipment like dust masks, eye protection and hearing protection
wherever necessary.
Soldering (brazing) tools Some ceramic kiln firebrick (the light porous kind-not the heavy kind)
to solder on. Check with local ceramicists for used bricks you can file
or grind off to use for this.
A Bernz-o-matic® type propane torch from the hardware store (approx.
$12.00) it is controlled by the angle it is held at. When the tank is
near vertical the flame is small, near horizontal it is larger. With a
little practice this is a great torch. These are great and very cheap.
Some white paste high temperature brazing flux (welders supply).
Several cheap watercolor brushes for painting flux on with for soldering.
Papermate® white out as a solder flow retardant to keep previously soldered
joins from coming apart when performing later soldering operations (let
air dry for 15 minutes before heating!)
Some high melting temperature silver solders for jewelry making, hard
and medium. Easy is generally used only for repair work.
Some low melting tin Stay-brite® solder and it's special flux from a
hardware store is useful for repairs and simple constructions where you
have a good contact surface area on the join.
A hot plate or crock pot for pickle to clean off oxides and flux residues.
(Pickle is an acidic compound which removes flux glazes and oxidized surfaces
from metals after soldering).
Sparex® jewellers pickling compound or swimming pool acid from the pool
store (approx. 1 teaspoon per 500 ml). The swimming pool acid is the same
chemical more or less; sodium bisulfate. Note that in a pinch a cup of
vinegar and a tablespoon full of table salt makes a very good cleaning
pickle as does pickling alum from the supermarket. (1 teaspoon of alum
to a quart or so of water).
Finishing tools A hand brass brush is used with a soapy water solution for satin finishes.
The soapy lubrication is essential for good results. You could try steel
wool too but I don't personally like it .
Some dishwashing liquid and household ammonia in hot water is used for
a degreasing solution to remove polishing compound residues and general
greases from fingers and so on. This is the jewellers secret formula for
cleaning jewelry; soak the piece in the hot solution a while, then scrub
with an old toothbrush to clean it. Don't clean emeralds or opals like
this as they may be damaged.
A stainless or Corning® pot and hot plate to warm the degreasing solution
in is good.
A spoon or a printmakers type burnishing tool is used for burnishing
edges and surfaces.
A Scotch-Brite® pad works for a satin finish (Janitors throw away the
centers of floor polishing pads which are the same type of material -
ask and they are free!)
A buffing wheel on a mounted electric hand drill or on a polishing motor
(a washing machine motor and tapered spindle) are great if you want the
bright shine one expects with jewelry.
Some tripoli and rouge (or Fabulustre® polishing compound instead of
the first two).
Some toothpaste or Old Dutch Cleanser® for satin finishes, perhaps some
commercial polishing pastes for brightness.
Some people like turtle wax or an equivalent for surface protection,
particularly on brasses, transparent auto enamel is good sometimes if
patinas are used.
Access to a sink or bucket or water and paper towel or dry hardwood
(not oak or pine) sawdust in a plastic container is used for drying metal
in after washing and rinsing it-dip the metal in alcohol, place in sawdust,
shake around and brush off. This results in spot free drying.
The most important adviceDon't put a mark in the metal unless you
want it there. Measure twice; cut once-half an hour of planning, layout
and checking saves two hours of repairs I hope this gives a good starting point for those who have been nervous
about working metals and encourages you to try out making your own jewelry
- it can be most rewarding especially when combined with your own gemstones
that you have cut and polished.
|