As with most Japanese metal coloring methods the techniques are metallurgically based rather than solution oriented; in the West we tend to use a myriad of coloring solutions and limited number of alloys; in Japan there are a limited number of coloring solutions and innumerable metal alloys which react differently in the same solution.... (1995) Complete Story
Niage is an important Japanese patina, and one of the most basic. It has been used as the base color on copper and copper alloys for centuries, and today it is also used as a final patina. As is true of all the recipes given here, these proportions are general guidelines, and experimentation is encouraged. A wide range of colors can be achieved by changing the concentration, proportions, or the time of exposure....
ISBN (2004) Complete Story
Japanese artists have contributed significantly by using their unique alloys in innovative combinations. Perhaps the best example of this is mokume-gane, a lamination process in which layers of various alloys are manipulated to create a rich pattern. In addition, Japanese work of many periods shows highly skilled inlay techniques where, again, the complex pallette of Japanese alloys is used to achieve subtlety and a controlled use of color.... (2004) Complete Story
The rich history of Japanese patinas is the result of hundreds of years of experimentation, innovation and tradition. This article covers some special Japanese Patinas; Wara-ibushi, Nuri-iro, Iroe-do, Ryuka (Sulfuration and Concentrate), Furubi, Kin-Furubi and alternative Furubi formulas.... (2004) Complete Story
It is impossible to pretend that a single description of tools, materials, and equipment will suit all needs. Obviously these elements will depend on the scale of the work you do, the layout of your studio, and the resources at your disposal. A sculptor working in large-scale bronze castings will have different needs from a jeweler.... (2004) Complete Story