The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Galleries | The BenchExchange | MetalCalc |
| Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | More...

If you benefit from what we're doing and want to give something in return, you can make a donation!

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
Advertise Here!
 
 
 
 

Library > Casting > Platinum Casting
 
Page: 1 2 
 
[748] Platinum Casting with Gemstones In Place
Platinum casting with gemstones in place has been the latest development before the end of the second millennium. It has been a world first to give fully successful results. The development of this new process required several years of uninterrupted experimentation, and in the spring of 1999 I obtained the first good results that encouraged me to continue the study.... (2004)
Complete Story

Show me more articles from: [Platinum Guild International]|[Hubert Schuster]
Releated Categories: [Platinum Casting]

 

[542] Platinum Casting: The Power of Process Control
It is widely known that platinum, the most noble of metals, is also the most challenging of metals. Platinum's high level of sensitivity to even the tiniest variation in processing was something we had experienced first hand and as most things of high value, had to be learned the hard way. We now maintain a controlled process with yields upwards of 95%. The beauty of a controlled process is that given the right tools and a high level of determination, anyone can do it.... (2003)
Complete Story

Show me more articles from: [Platinum Guild International]|[Helmut F. Frye, Ph.D. Timothy L. Donohue]