The annealed metal is placed in a sandwich between soft 'pusher' paper and a hard paper which will serve as a monoprint paper die to emboss the metal sheet. The metal may be pre-polished.... (1990) Complete Story
For all metal coloring and electroplating a clean metal surface is essential. The cleaning process must remove mineral oils, organic oils and greases as well as traces of chemicals on the surface. It must remove oxidation which might interfere with the metal coloration or plating adhesion and it should possible activate or roughen the metal surface to better receive the treatment.... (2002) Complete Story
In the twentieth century there can be little doubt that electroplating is the best way to develop a gold coating on a metal object. It provides successful results in many colors and can be adapted to one-of-a-kind or mass production. Knowing this, it might seem peculiar to devote the following section to the ancient art of fire gilding. It is more time consuming than modern methods, it requires more material, there is a greater risk of failure, and it is a health risk unless performed under ventilation. Why then should it be included?.... (2001) Complete Story
Using 1 inch by 11 inch belts with a 4.25-inch working surface, this sander fits onto a flex-shaft with a quick-release collar. It can be clamped onto a table or bench and is adjustable to many angles. An optional mounting attachment is available for use with the GRS Benchmate. The sander comes with five assorted belts in a variety of grits from very coarse to very fine. Why it´s one of Pat Pruitt´s coolest tools.... (2011) Complete Story
Double is a German word of french origin meaning rolled gold or gold fill material. I use it for the gold-fill material described here to differentiate it from the commercially produced sheet. Hand made double has different qualities than the manufactured metal. It is far less perfect, its finished size is limited by one's workshop facilities and counting hours it costs more per square centimeter....
(1985) Complete Story
Would you like to reach Members of the Ganoksin Project to educate
them about the wonderful array of supplies, services and products
you have to offer?
Please request a copy of the Ganoksin Media Kit if you would like
more indepth information regarding Ganoksin's advertising services.