[254] The Earliest Cloisonne Enamels from Cyprus
An island in the eastern Mediterranean, with a history of more than 8000 years, Cyprus was one of the earliest producers of copper in the world, had a flourishing metal industry and during the "Golden Age" of Cyprus, the island enjoyed a high level of prosperity. This brought a great number of settlers and craftsmen from neighboring countries.... (1989)
Complete Story

Show me more articles from: [Glass on Metal]|[Dr. Panicos Michaelides]
Releated Categories: [Jewelry History]|[Enameling History]|[Cloisonne Enamel]