Cast hinges are a very important part of much production jewelry work, partly because hinge assembly on such pieces is reduced to inserting the hinge pin and so provides a very fast linkage system ideal for cast objects. We are primarily speaking here of lost wax investment casting. If you look at any trade magazines you will find many examples of cast hinges in the advertisements....
(1997) Complete Story
Firescale has been the scourge of sterling silver casters since the first silver was poured into a mold. It has been a thorn in the side of silver fabricators. Fortunately there are ways to prevent fire scale while silver soldering. This paper describes a simple, inexpensive method of preventing fire scale during vacuum casting.... (2005) Complete Story