[373] Shortening Bracelet Using Pulse-arc-Welding Techniques
This Charles and Colvard created moissanite (hereafter referred to as moissanite) and two-tone karat gold in-line bracelet requires shortening by two links. The bracelet is held together by a heavy link-wire that's wrapped around an open portion of the adjacent link and permanently joined, giving the bracelet maximum flexibility. Below is a procedure for shortening, reassembling and permanent welding of the link using pulse-arc-welding technology..... (2004)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories: [Fusing & Welding]|[Repairs]

 

[374] Sizing a Platinum Ring Using Pulse-arc Welding Technology
Sizing and torch welding a platinum ring with diamonds channel set down the shank could be risky to the diamonds. Use of a Pulse-arc Welder for this welding job will eliminate the risk and potential damage.... (2004)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories: [Fusing & Welding]|[Repairs]

 

[915] Speedwire Saves Time and Improves Laser Welding Accuracy
When Glenn Manning of Manning Jewelry in Foley, Alabama, bought his first laser welder almost a decade ago, he thought it was a magnificent piece of equipment. But He soon realized that while the laser welder had many advantages over traditional soldering, it was troublesome to handle the wire used in the process. Mannings solution, a laser welding wire dispenser that he calls Speedwire, solves those problems and more-and its getting rave reviews from the handful of people in the jewelry industry who have had the chance to try it.... (2010)
Complete Story

Show me more articles from: [AJM]|[Shannon Cournoyer Brown]
Releated Categories: [Fusing & Welding]
ISBN: B00006K39S

 

[853] The PUK Generation 3 - Fine Welding Devices
For two years now, the manufacturer Lampert has been cooperating with the Laboratory for Welding Technology and Thermal Treatment at the Polytechnic College in Wrzburg-Schweinfurt. Test series and fundamental scientific research is applied in order to continue the technological development. And now the Generation 3 is well on its way to conquering the studios. The new device series consists of three models that will appeal to beginners, ambitious users and also professional. They offer numerous new features under the names PUK3 basic, PUK3 Professional and PUK3 Professional plus. (2007)
Complete Story

Show me more articles from: [GZ Art+Design]|[Axel Henselder]
Releated Categories: [Fusing & Welding]|[Shop Machines]
ISBN: B00007B9ED

 

[601] Tool Modifications for Tack-, Fusion- and Pulse-arc-Welding Technology
Proper holding and firm contact between parts during tack-, fusion- and pulse-arc-welding is essential. Aside from pieces not meeting properly, most destructive discharges result from poor holding and/or insufficient contact. A destructive discharge causes damage to the parts being assembled. The tools supplied with the Tack II and Pulse-Arc Welders provide good holding devices for the majority of jobs you will encounter. With minor modifications and skillful use of these tools and the development of tools you may design and fabricate, you will minimize destructive discharges. Here are some examples of tool modifications you may find useful.... (2005)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories: [Fusing & Welding]

 

Page: 1 2 3 4 5 6 7 8 9 10 


 
Donate! If you believe in what we're doing, you can help!