The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Galleries | The BenchExchange | MetalCalc |
| Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | More...

If you benefit from what we're doing and want to give something in return, you can make a donation!

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
Advertise Here!
 
 
 
 

Library > Surface Manipulation > Niello
 
Page:
 
[84] Niello Work
Niello is a deep black metal mixture that is fused onto metal for decorative effect. Though worked on three-dimensional objects, the effect might be considered graphic because it relies primarily on shape and pattern. The contrast of the lustrous black inlay against either matte or polished metal is striking and has earned niello a special place in the arsenal of decorative techniques.... (2001)
Complete Story

Show me more articles from: [The Theory and Practice of Goldsmithing]|[Prof. Dr. Erhard Brepohl]