Niobium has many properties that make it an excellent candidate for fabricated parts. Of particular interest to jewelry manufacturers and designers are niobium's hypoallergenic nature, formability, and the broad range of anodized colors that can be rendered on its surface. It is considered hypoallergenic and safe to wear for even those most sensitive to metal allergies..... (2004) Complete Story