| [239] Stone Setting - A Crowning Achievement |
Often jewelers are called upon to hand fabricate a crown to fit a stone. This is necessary when either the stone is a non-standard shape, or the crown needs to fit a particular design. Although one will seldom hand fabricate a simple round basket crown, constructing one gives the jeweler the basic knowledge and understanding of crown construction needed when creating a more advanced crown.... (2003)
 Complete Story |
| Show me more articles from: [BWSimon]|[Bradney W. Simon] |
| Releated Categories: [Bench Tips & Tricks]|[Stone Setting] |
|
| [676] Stone Setting Considerations - Installment 1 |
One of the most challenging and technically difficult of the activities involved in the creation of jewelry is the setting of gemstones. Setting the gemstones is often the final step in the entire process of making a piece of jewelry. Not only is this procedure exacting and critical in its application, it is also both taxing and stressful to the body and mind of the setter.... (2005)
 Complete Story |
| Show me more articles from: [Ganoksin]|[Michael David Sturlin] |
| Releated Categories: [Stone Setting] |
|
| [139] Stonesetting: Engraved bezel with vertical walls |
Stonesetting has been a part of goldsmithing for as long as people have worked in precious metals. Perhaps the oldest and most used setting has been the bezel. The simplest form of the bezel is a ring of metal fitting the circumference of the enclosed cabachon or tapered material soldered onto a base plate. The stone fitted inside, and the metal is pushed, burnished or hammered towards the stone.... (1977)
 Complete Story |
| Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain] |
| Releated Categories: [Stone Setting] |
|
| [873] The Nuances of Small Stakes and Anvils |
Shaping a bezel on stakes is a process of forming the metal by stretching. First the metal is bent with pliers to fit the gem, forming a shape smaller than the stone while following its contour. The gauge of the sheet metal chosen is slightly thicker than the final result. As the process unfolds, the metal is plannished (hammered) on small stakes, causing the metal to conform to the stake as it stretches. If the gemstone and the shape of the stake are the same, a very accurate bezel can be made with a minimum of time. The advantages of this technique become obvious to the craftsperson that uses creatively shaped stones or gems that do not conform to the bezel mandrels on hand.... (2008)
 Complete Story |
| Show me more articles from: [Ganoksin]|[William Fretz] |
| Releated Categories: [Small Tools]|[Stone Setting] |
|
| [140] Tube setting - an introduction to setting |
Tube setting is a simple method of setting that can take as little as five minutes or less per setting given a specified stone size and a suitable tube to fit the stone. The setting is visually clean, has a professional look to it and can be done with a minimum of tools. Note that setting is usually done on jewellery that is finished. Setting is then the last step in the process of making the piece.... (1990)
 Complete Story |
| Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain] |
| Releated Categories: [Stone Setting] |
|
|
|
|
|
| |