The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Galleries | The BenchExchange | MetalCalc |
| Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | More...

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
 
 
 

Back
Articles by Jurgen J. Maerz
Page: 1 2 3 
 
[540] Making a Forged Platinum Pearl Ring – A Step by Step Project
This project will teach welding, soldering and forging techniques. The ring is a handsome, plain design and can be applied to many applications. To make this ring, you will need.... (2005)
Complete Story

Show me more articles from: [Platinum Guild International]|[Jurgen J. Maerz]
Releated Categories:[Platinum Fabrication]

 

[264] Platinum - Bench Tricks
This project is dedicated to bench tricks that make working with platinum-or working at the bench in general-easier. This is the first installment of a periodic Platinum Bench series.... (2003)
Complete Story

Show me more articles from: [AJM]|[Jurgen J. Maerz]
Releated Categories:[Bench Tips & Tricks]|[Platinum Fabrication]
ISBN: B00006K39S

 

[309] Platinum - Durability vs. Scratching
There is a major difference between durability and scratch resistance. Platinum is very durable. When scratched, the scratch actually displaces the metal, leaving ridges on the edges of the scratch. This is where durability comes in. Whereas other precious metals, if scratched, lose metal, and thus wear down, Platinum does so at a much slower rate.... (2002)
Complete Story

Show me more articles from: [Platinum Guild International]|[Jurgen J. Maerz]
Releated Categories:[Metals]|[Platinum Fabrication]|[Polishing]

 

[519] Platinum Alloy Applications for Jewelry
Today, platinum is enjoying its renaissance. In the U.S., platinum consumption has risen by more than 700% since 1990. More jewelers are carrying platinum jewelry, and consumers are becoming more aware of the most noble of all metals. Many jewelers are still confused as to the platinum alloys available, their application and purpose, this paper will attempt to clear up some of these issues.... (2000)
Complete Story

Show me more articles from: [Platinum Guild International]|[Jurgen J. Maerz]
Releated Categories:[Metallurgy]

 

[745] Platinum Alloys - Features and Benefits
In this presentation I attempted to provide you with information on platinum alloys to help you make an informed decision as to which alloy to employ for your manufacturing venture. There are several alloys I did not mention, mainly because they are experimental and have not found their way into the main stream. An alloy is chosen for its capability, ease of recycling and many other criteria. It must be user friendly, scratch and bend resistant and hold your stones securely. It is further of importance that it can be finished with few or no problems and hold a shine. These alloys that can do all this are here. They are on the market and can do just what you are looking for. It is sometimes just a matter of breaking old habits to see a major improvement in your product.... (2004)
Complete Story

Show me more articles from: [Platinum Guild International]|[Jurgen J. Maerz]