Amber begins as resin exuded from trees millions of years ago. All known deposits of amber come from various tree species which are now extinct. Baltic amber was produced by a tree called Pinites succinifer, a tree sharing many characteristics of the currently living species Pseudolarix. In appearance it would have looked something similar to a pine or spruce tree.... (1998) Complete Story