The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Galleries | The BenchExchange | MetalCalc |
| Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | More...

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
 
 
 

Back
Articles by Chris Corti
Page: 1 2 
 
[737] Recent Developments in Electroforming
Electroforming is an old, established technology and, in its original form, it was a bit cumbersome to use. However, as with other jewelry technologies, it has made great strides over the last decade and is now a much easier and quicker process. In this article, I shall focus on gold, but other precious metals can also be electroformed successfully.... (2003)
Complete Story

Show me more articles from: [AJM]|[Chris Corti]
Releated Categories:[Plating & Electroforming]
ISBN: B00006K39S

 

[219] Tarnishing Of Gold Jewellery And Black Skin Smudging
Tarnishing is superficial corrosion of the carat gold surface and is evident by a usually dark discolouration - the tarnish film. Pure gold, of course, is not susceptible to tarnishing and this property is generally not greatly reduced by alloying to carat golds as long as the gold content is high enough.... (2003)
Complete Story

Show me more articles from: [The World Gold Council]|[Chris Corti]